| ltem | Specifications |
| Viscosity | 40000~200000 mPa.s |
| Substitution degree (MS) | 1.8-2.2 |
| Ash content (%) | ≤5% |
| Maximum moisture content (%) | ≤5% |
| PH (1% solution, 20 ℃) | 6-8 |
01.
Alkalization treatment:
Treat cellulose with NaOH solution to form alkali cellulose Swelling cellulose facilitates subsequent reactions
02.
Etherification reaction:
Add etherification agent (such as chloromethane) under alkaline conditions Substitution reaction occurs to generate cellulose ether
03.
Washing and neutralization:
Adjust the pH to neutral, wash away by-products and residual reagents
04.
Drying and crushing:
Obtain the final product
Our Certificates
We adhere to innovation and research and development, committed to improving user satisfaction.
● Has over 100 patents at home and abroad, including 47 invention patents and 30 utility patents
● National Postdoctoral Cellulose Ether Workstation
● ISO 9001, IS0 45001, IS050001, IS0 14001, FSSC22000, HLAL/KOSHER and other certifications